Typical Tensile Properties
ISO As welded | ||
Elongation | Tensile Strength | Yield Strength |
35 % | 780 MPa | 500 MPa |
Typical Charpy V-Notch Properties
ISO As welded | |
Impact Value | Testing Temperature |
70 J | 20 °C |
50 J | -196 °C |
Typical Weld Metal Analysis %
Mn | Mo | C | Nb | Si | Ni | Cr | Fe |
0.2 % | 9.3 % | 0.03 % | 3.3 % | 0.4 % | 62.8 % | 21.7 % | 2.0 % |
Deposition Data
Diameter | Current | Deposition Rate | Fusion time per electrode at 90% I max | kg weld metal/kg electrodes | Number of electrodes/kg weld metal | Voltage |
2.5 x 300 mm | 55-75 A | 0.9 kg/h | 40 sec | 0.55 kg | 100 | 23 V |
4.0 x 350 mm | 80-140 A | 1.9 kg/h | 57 sec | 0.58 kg | 33 | 27 V |
3.2 x 350 mm | 65-100 A | 1.4 kg/h | 52 sec | 0.56 kg | 49 | 25 V |
5.0 x 350 mm | 120-170 A | 2.1 kg/h | 72 sec | 0.58 kg | 21 | 24 V |
Approvals: | CE, EN 13479, DNV-GL, -H5, VdTÜV, 12414 |
Classifications: | SFA/AWS A5.11, ENiCrMo-3, EN ISO 14172, E Ni 6625 (NiCr22Mo9Nb) |
Approvals are based on factory location. Please contact ESAB for more information.
Alloy Type: | Ni-based CrMoNb |
Coating Type: | Basic |
Ferrite Content: | FN 0 |
Welding Current: | DC+ |